Gas-Fired Oven is used for curing rubber hose.
2014-06-03 14:30:56| Industrial Newsroom - All News for Today
With overall length of 77 ft 8 in., which includes 64 ft heated length, gas fired oven is used to cure internal rubber lining of hose prior to bonding with outer-most hose material. Oven operates at 650°F and can reach 700°F max temperature. Along with part conveyance via 3 separate conveyor levels to ensure proper curing time, features include 1.5 min dwell time, 100 fpm line speed, side access doors for maintenance, heat-loss hoods, and circulation ducts. This story is related to the following:Rubber Curing Ovens |
Tags: rubber
oven
hose
curing